Facility ID: 44432LBCFN230WM
Facility Name and Address: ALBCO FOUNDRY INC 230 W MAPLE ST LISBON, OH 44432 Parent Company: Industry: Other Nonferrous Metal Foundries (except Die-Casting) (331529) Chemical: Lead compounds Reports: View TRI Facility profile report for this facility View TRI Form R submissions by this facility |
|
*You can navigate within the map with your mouse. |
Production Related Waste Management for Selected Chemical
lchemid=N420
Chart Options1: |
Waste Management Comparison -
Display facility comparison report for this industry and chemical
Pollution Prevention Activities for Selected Chemical
Reporting Year | Section 8.10: Newly Implemented Source Reduction Activity | Section 8.10: Methods to Identify Activity | Section 8.11: Optional Pollution Prevention Information* |
---|---|---|---|
2022 |
Source Reduction:: S03: Substituted raw materials, feedstock, or reactant chemical
|
Methods to Identify SR Opportunities: T11: Other
Barriers: B1-No Information B1 - Insufficient capital to install new source reduction equipment or implement new source reduction activities/initiat |
S03: Continue to navigate customer to a low/no lead substitute |
2021 |
Source Reduction: Source Reduction - Replaced all dust collector filters to increase capture. |
||
2020 |
Other Barriers to Source Reduction - We continue to promote no/low lead product to our customers with safer alternative material. Other Environmental Practices: Recycling - We continue to find opportunities to recycle for material reclaim. |
||
2019 |
Other Environmental Practices - We have installed a fume/dust collection at our main melt furnace.20+ years prior was a stack.
Source Reduction: Source Reduction - We continually educate our customers about the use oflow/no lead alternatives.Industry standard for bearing bronze is C932 which we do not process.We offer the Low/No Lead option of C903. |
||
2018 | Other Environmental Practices - Albco is currently working on reducing fume escape by eliminating piping fume draw to stack and rerouting to a collection point for recycling. | ||
2017 |
Source Reduction: Source Reduction - Many old blueprints specify C932/C937 leaded alloy for the product.We have been converting to the no lead tin bronze as an alternative. |
||
2016 |
Source Reduction: Source Reduction - Albco Foundry continues to promote alternative no lead non-ferrous material for our customers applications. |
||
2014 | Source Reduction - We are educating our customers to use other alternatives other than current metals for reduction. As a result there has been a 24% decrease of claimed element. | ||
2005 |
Source Reduction:: W42: Substituted raw materials
|
Methods to Identify SR Opportunities: T01: Internal pollution prevention opportunity audit(s)
Methods to Identify SR Opportunities: T03: Materials balance audits |